Mechanical Properties Metric English Comments
Shear Strength 15.9 MPa
2300 psi
Tensile Shear Strength; ASTM D1002
Protective Coating PC-Clear™ Clear Liquid Epoxy
PC-Clear™ is a completely clear liquid epoxy formulated to remain clear during and after its curing time. PC-Clear™ is very durable and flexible making it unlike many liquid epoxies. Uses include..
Shear Strength 15.9 MPa
2300 psi
Cured, tensile, Al/Al
Resin Technology Group EN 139-2 UV Gellable, Low Temperature Cure, One-Component Epoxy Adhesive
EN 139-2 is a UV gellable, one-component epoxy based adhesive system designed to provide cure at temperatures as low as 80°C. This one-part adhesive gels to a tack-free, low strength polymer upon e..
Shear Strength 15.9 MPa

@Temperature 316 °C
2300 psi

@Temperature 600 °F
Greene Tweed Arlon® 1000 Polyketone
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..
Shear Strength >= 15.9 MPa
>= 2300 psi
Bond, Al to Al
Master Bond EP45HTAO Heat Resistant Epoxy for Structural Bonding
Description: Master Bond Polymer Compound EP45HTAO is a two component thermally conductive epoxy compound for high performance structural bonding, and casting. It is suitable for applications where ..
Shear Strength >= 15.9 MPa
>= 2300 psi
Tensile lap, Al/Al
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System
Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi..
Shear Strength >= 15.9 MPa
>= 2300 psi
Bond, Al to Al, after 30 days water immersion
Master Bond Supreme 45HTND Toughened Epoxy for Structural Bonding
Description: Master Bond Polymer Adhesive SUPREME 45HTND is a two component epoxy adhesive featuring a balance of shear and peel strengths for high performance structural bonding suitable for applic..
Shear Strength 15.9 MPa
2300 psi
Overlap, Al/Al
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
Shear Strength 15.9 MPa
2300 psi
Overlap, Etched Aluminum, 30 days tap water @ RT
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
Shear Strength 15.9 MPa
2300 psi
Overlap, Abraded Aluminum, Initial
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
Shear Strength 15.9 MPa
2300 psi
Overlap, Aluminum Oakite degrease
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 15.9 MPa
2300 psi
Overlap, Galvanized Aluminum (MEK/abrade/MEK), Adhesive Failure; ASTM D1002
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..
Shear Strength 15.9 MPa
2300 psi
3M Scotch-Weld™ DP601 Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon..
Shear Strength 15.9 MPa
2300 psi
3M Scotch-Weld™ DP601NS Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon..
Shear Strength 15.9 MPa
2300 psi
Overlap, 304 Stainless Steel (1/32" thick), Cohesive Failure
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 15.9 MPa
2300 psi
Overlap, Etched Al, Salt Spray at RT for 14 days
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
Shear Strength 15.9 MPa
2300 psi
Overlap, Steel; ASTM D1002-64
3M Scotch-Weld™ CA4 Instant Adhesive
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Fast setting for a variety of plastics and rubbers.Information provided by 3M
Shear Strength 15.9 MPa
2300 psi
Overlap, Etched Aluminum, 30 days tap water @ RT
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M