Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 94.5 MPa @Temperature 23.9 °C |
13700 psi @Temperature 75.0 °F |
Short-Beam, Dry; ASTM D2344 |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, G30-700 Uni-Tape Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Shear Strength | 94.4 MPa | 13700 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Shear Strength | 94.4 MPa | 13700 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Shear Strength | 94.4 MPa | 13700 psi | ILSS; EN2563 |
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/35%/UD134/AS7-12K Fiber: AS7, Weave: UD, 134 g/m2Information provided by HexCel |