Mechanical Properties Metric English Comments
Shear Strength 9.10 MPa
1320 psi
Lap
Epoxy Technology EPO-TEK® H31 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H31 is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electronic..