Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 8.62 - 11.0 MPa | 1250 - 1600 psi | |
ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works. |
|||
Shear Strength | 8.62 - 10.3 MPa | 1250 - 1500 psi | |
ITW Plexus Plexusâ„¢ MA556 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Information provided by Illinois Tool Works.. |
|||
Shear Strength | 8.62 - 10.7 MPa | 1250 - 1550 psi | |
ITW Plexus Plexusâ„¢ MA557 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Long working time, non-sagging, excellent g.. |
|||
Shear Strength | 8.62 - 10.3 MPa | 1250 - 1500 psi | |
ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works. |
|||
Shear Strength | >= 8.62 MPa | >= 1250 psi | Bond, Al to Al |
Master Bond EP76M-1R Nickel Conductive Epoxy Adhesive Description: Master Bond Polymer System EP76M-1R is a two component, nickel filled, electrically conductive adhesive for high performance bonding formulated to cure at room temperature or more rapid.. |
|||
Shear Strength | >= 8.62 MPa | >= 1250 psi | Plate Shear (Beam shear for 12.0 pcf products), L Direction, min |
Hexcel® HexWeb® CR III 1/8-5052-.003 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 8.62 MPa | >= 1250 psi | Plate Shear (Beam shear for 12.0 pcf products), L Direction, min |
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.0037 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 8.62 MPa | 1250 psi | Lap |
Epoxy Technology EPO-TEK® E4110-PFC Electrically Conductive Epoxy Product Description: EPO-TEK®E4110-PFC is a two-component, silver filled, electrically conductive adhesive designed for semiconductor IC packaging and general electronic assembly. It is a thixotr.. |
|||
Shear Strength | 8.62 MPa | 1250 psi | CRS Overlap, 100% RH at 49°C |
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Shear Strength | 8.62 MPa | 1250 psi | Overlap, Abraded Aluminum, 30 days tap water @ RT |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 8.62 MPa | 1250 psi | Overlap, Lexan, Cohesive Failure |
3M Scotch-Weld™ DP8010 Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl.. |
|||
Shear Strength | 8.62 MPa | 1250 psi | Overlap, 71°C 100% RH for 14 days, Mixed Mode of AF&CF |
3M Scotch-Weld™ DP810NS Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 8.62 MPa @Temperature 32.0 °C |
1250 psi @Temperature 89.6 °F |
Overlap, Oak, 90% RH, Substrate/Adhesive Failure |
3M Scotch-Weld™ Thin Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 8.62 MPa @Temperature -55.0 °C |
1250 psi @Temperature -67.0 °F |
Overlap |
3M Scotch-Weld™ DP100 FR Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 FR is a two-part flame retardant (self-extinguishing) version of Scotch-Weld DP100. It meets the UL94 V-O Burn Test requirements and has a work life of 4-8 mi.. |
|||
Shear Strength | 8.62 MPa | 1250 psi | Overlap, Acrylic |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 8.62 MPa @Temperature 81.0 - 83.0 °C |
1250 psi @Temperature 178 - 181 °F |
Minimum MMM-A-132 Requirement |
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |
|||
Shear Strength | 8.62 MPa | 1250 psi | Overlap, Abraded Aluminum, 30 days tap water @ RT |
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |