Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 1.50 MPa | >= 218 psi | Steel Pins & Collars; ISO 10123 |
Palm Labs Adhesives TURBO SEAL SERIES 55 BROWN FINE THREADS THREAD SEALANT TURBO SEAL SERIES 65 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures quickly in the absence of air between.. |
|||
Shear Strength | 1.50 MPa | 218 psi | Plate Shear, W direction |
Hexcel® HexWeb® CRF-1/4-ACG-.003-15.2 Chromate free ACG® Honeycomb Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app.. |
|||
Shear Strength | 1.50 MPa | 218 psi | Lap |
Epoxy Technology EPO-TEK® T7109-18 Electrically Insulating Epoxy Paste Material Description: A flexible, electrically insulating epoxy paste designed for low stress and heat dissipation applications. Alternative to EPO-TEK® T7109-17.Information Provided by Epoxy Tec.. |
|||
Shear Strength | 1.50 MPa | 218 psi | |
Dow Corning 3-6006 SILICONE ADHESIVE/SEALANT One-part, fast cure silicone adhesive.Information provided by Dow Corning |
|||
Shear Strength | 1.50 MPa | 218 psi | Overlap, Maple, 50% RH |
3M 4200 Marine Adhesive/Sealant Fast Cure A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds to wood, gelcoat and fiberglass. It forms watertight, weather-resistant seals on joints an.. |
|||
Shear Strength | 1.50 MPa | 217 psi | Overlap, Acrylic, 50% RH |
3M 5200 Marine Adhesive/Sealant 3M™ Marine Adhesive/Sealant 5200 is a one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds. It has excellent adhesion to wood, gelcoat and fiberglass. It for.. |
|||
Shear Strength | 1.50 MPa | 218 psi | Typical; ASTM C273 |
Parabeam Industrie ParaTank 3 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |