Polymer Property : Shear Strength = 1.40 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 1.40 MPa
203 psi
ASTM C273
SABIC Innovative Plastics ULTEM Foam XP110 PEI
ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The ..
Shear Strength >= 1.40 MPa
>= 203 psi
ISO 1922
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Shear Strength 1.40 MPa
203 psi
Overlap, Aluminum, 50% RH
3M 5200 Marine Adhesive/Sealant Fast Cure
A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds with excellent adhesion to wood and fiberglass. Forms watertight, weather-resistant seals ..
Shear Strength 1.40 MPa
203 psi
average; ISO 1922
3A Composites Core Materials AIREX® R82.110 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines outstanding fire resistance with low smoke and toxicity, along with excellent dielectric properties. It has a good strength to ..
Shear Strength 1.40 MPa
203 psi
Plate Shear, L direction
Hexcel® HexWeb® CRF-1/4-ACG-.002-3.4 Chromate free ACG® Honeycomb
Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app..