Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus | 480 MPa | 69600 psi | ASTM D638 |
SABIC R40039E Medium Density Polyethylene for Rotational Molding Product Description: R40039E is a Medium Density Polyethylene grade designed to provide excellent mechanical properties with high rigidity, toughness, gloss and low warpage. R40039E is UV stabiliz.. |