Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus 483 MPa
70000 psi
0.5 in/min; ASTM D790
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade
ApplicationsMicrothene MP574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items. MP574189 is 16 mesh pow..
1% Secant Modulus 483 MPa
70000 psi
ASTM D882
Total PPR 8650 Polypropylene, Random Copolymer
ATOFINA 8650 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The low melting point of ATOFINA 8650 makes it an excellent heat seal layer for orie..