Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus | 174 MPa | 25200 psi | ASTM D638 |
SABIC 318CN Linear Low Density Polyethylene for Wire & Cable Product Description: 318CN is a Linear Low Density Polyethylene natural resin for wire and cable applications. It contains a low level of antioxidants and does not contain any slip or antiblock a.. |