Mechanical Properties Metric English Comments
1% Secant Modulus >= 170 MPa
>= 24700 psi
ASTM D638
SABIC HP7022 Low Density Polyethylene for Injection Molding
Product Description: HP7022 is a Low Density Polyethylene offering a unique combination of consistent processability, flexibility and toughness. Articles manufactured from HP7022 exhibit excellent..