Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 30.0 g/micron | 762 g/mil | ISO 7765/1 |
Borealis Borstar® FB1460 HDPE for Film Borstar FB1460 is a high-density polyethylene film grade, which combines superior physical properties with excellent processability. Due to the high density, the material properties are best utiliz.. |
|||
Dart Drop | 30.0 g/micron | 762 g/mil | ASTM D1709A |
Westlake Hifor LT74107-F Polyethylene Film, Using Energx Technology Services
(discontinued **) Hifor LT74107-F polymer is a high strength and good clarity polyethylene designed for blown film extrusion that contains medium slip, high antiblock and high processing aid additives. Films produced.. |
|||
Dart Drop | 30.0 g/micron | 762 g/mil | ASTM D1709 |
ExxonMobil Exceed™ 2018EB Blown Film Resin
(discontinued **) Exceed 2018EB resin is an ethylene based polymer produced with metallocene single site catalysts using ExxonMobil Chemicals Exxpol® Technology. The higher melt index makes this polymer ideally sui.. |