Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 2.83 g/micron | 71.9 g/mil | ASTM D1709 |
SABIC 218 Series Linear Low Density Polyethylene for Blown Film Product Description: 218 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. They are easy to process giving good tensile properties, impact strength a.. |
|||
Dart Drop | 2.83 g/micron | 71.9 g/mil | ASTM D1709 |
SABIC 726 Series Linear Low Density Polyethylene for Blown Film Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher .. |