Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 7.350 g/micron | 186.7 g/mil | ASTM D1709 |
ExxonMobil ESCOR™ AT 310 Cast Film Resin
(discontinued **) ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo.. |