Polymer Property : Dart Drop = 52.0 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 2.05 g/micron
52.0 g/mil
F50; ASTM D1709
ExxonMobil Escorene® LD-113 LDPE General Purpose Packaging Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin that offers a good balance of toughness, drawdown capability, stiffness and clarity. LD-113 exhibits good machinability in..
Dart Drop 2.05 g/micron
52.0 g/mil
F50; ASTM D1709
ExxonMobil Escorene® LD-134 LDPE Packaging Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo..