Polymer Property : Dart Drop = 518 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 20.4 g/micron
518 g/mil
F-50 at 26 in.; ASTM D1709
Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Dart Drop 20.4 g/micron
518 g/mil
F-50 at 26 in.; ASTM D1709
Chevron Phillips Dynex™ D508A Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Dart Drop 20.4 g/micron
518 g/mil
F-50 at 26 in.; ASTM D1709
Chevron Phillips Dynex™ D508A7 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Dart Drop 20.4 g/micron
518 g/mil
F-50 at 26 in.; ASTM D1709
Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..