Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | >= 19.7 g/micron | >= 500 g/mil | F50; ASTM D1709 |
ExxonMobil Exceed™ 350D60 LDPE/Hexene Tough Premium Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D60 resin have outstanding tensile, impact streng.. |
|||
Dart Drop | 19.7 g/micron | 500 g/mil | Blown Film at 1 mil; ASTM D-1709 |
Chevron Phillips MarFlex® 7105D Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPE Appl.. |