Polymer Property : Dart Drop = 46.0 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 1.81 g/micron
46.0 g/mil
2.5 BUR; ASTM D1709
Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film
This LDLPE is tailored for applications that require:Good processabilityGood melt strengthGood drawdownGood strengthSatin finishGood MD & TD shrinkageGood contact clarity and lower gel contentTypica..