Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 16.4 g/micron | 417 g/mil | F-50 at 26 in.; ASTM D1709 |
Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart drop impact, hot-tack and heat seal properties, good drawdown, can b.. |