Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop = 4.50 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 4.50 g/micron
114 g/mil
ASTM D1709
SABIC 518N Linear Low Density Polyethylene for Blown Film
Product Description: 548N is a fractional melt index Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resin yield outstanding toug..
Dart Drop 4.50 g/micron
114 g/mil
ASTM D 1709/A
NOVA Chemicals Surpass® FPs225-A Octene Copolymer sLLDPE Film Resin
FPs225-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without ..
Dart Drop 4.50 g/micron
114 g/mil
ASTM-D1709 (Method B)
Braskem TN2020 EVA General Film Copolymer
TN2020 is an Ethylene-Vinyl Acetate (EVA) copolymer developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Multilayer structures..
Dart Drop 4.50 - 29.0 g/micron
114 - 737 g/mil
Average value: 10.5 g/micron Grade Count:20
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum..
Copyright © lookpolymers.com All Rights Reserved