Mechanical Properties Metric English Comments
Dart Drop 4.45 g/micron
113 g/mil
ASTM D1709
Westlake EMAC® EF598AA 9% Ethylene-Methyl Acrylate Copolymer
Clarity optics, excellent drawdown, excellent machinability, good TD heat shrinkage and excellent toughness. Uses include food packaging tie layers, heat seal layers, extrusion coating, cast film, ..
Dart Drop 4.45 g/micron
113 g/mil
F50; ASTM D1709
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su..