Polymer Property : Dart Drop = 3.10 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 3.10 g/micron
78.7 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips 5554-D LDPE High Clarity, Medium Impact, Low Slip Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Excellent Clarity, Good Impact Strength, Good Sealability, Low SlipApplications:Food Packaging, Case Shrink Wrap, LaminationsProcessing Conditions: Extruder 6..
Dart Drop 3.10 g/micron
78.7 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips 5758 LDPE High Clarity, High Impact Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: High Clarity, Excellent Impact Strength, Medium Slip, Medium Antiblock, Moderately High Coefficient of Friction, Easy Openability of BagsApplications:Case Shr..
Dart Drop 3.10 g/micron
78.7 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips 5754 LDPE High Clarity, High Impact Film Resin for General Purpose Packaging
Resin Type: HomopolymerCharacteristics: Excellent Impact Strength, High Clarity, Medium Slip, Medium Antiblock, Low Coefficient of Friction, Good OpenabilityApplications:Heavy Produce Bags, Frozen F..
Dart Drop 3.10 g/micron
78.7 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips MarFlex® 5755 LDPE High Clarity, High Impact Film Resin
Resin Type: HomopolymerCharacteristics: High Clarity, Excellent Impact Strength, Medium Slip, High Antiblock, Moderately High Coefficient of Friction, Excellent ProcessabilityApplications:Case Shrin..
Dart Drop 3.10 g/micron
78.7 g/mil
ASTM D1709A
Eastman D4036-F Polyethylene  (discontinued **)
D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener..