Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 9.84 g/micron | 250 g/mil | ASTM D1709 |
Formosa Plastics Formolene® E905 Film HDPE
(discontinued **) HMW-Bimodal ResinApplications: T-shirt bags, trash can liners, heavy duty bagsFormolene E905 is a high molecular weight grade of HDPE with well-balanced strength in both the machine (MD) and transve.. |
|||
Dart Drop | 9.84 g/micron | 250 g/mil | ASTM D1709 |
Westlake EF444 4.7% Ethylene Vinyl Acetate Copolymer
(discontinued **) Excellent haze and gloss, excellent impact strength and very good sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, section 177.. |
|||
Dart Drop | 9.84 g/micron | 250 g/mil | ASTM D1709 |
Metabolix M-vera™ B5010 Film Grade Compostable Bioplastic For use in tough, certified compostable film and bag applications. Mvera B5010 offers a wide range of attractive traits—excellent tear and puncture toughness, excellent seal strength, good prin.. |
|||
Dart Drop | 9.84 g/micron | 250 g/mil | ASTM D1709 |
Westlake EF601 Low Density Polyethylene Westlake EF601 is a fractional melt LDPE with excellent toughness. It is suggested in heavy duty films and shipping sacks, and in industrial shrink applications. It can be used as a bubble stabilize.. |
|||
Dart Drop | 9.84 g/micron | 250 g/mil | ASTM D1709 |
Westlake Elevate™ EF439 4.0% Ethylene Vinyl Acetate Copolymer Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio.. |
|||
Dart Drop | 9.84 g/micron | 250 g/mil | ASTM D1709 |
Westlake Hifor Xtreme SC74838 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74838 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and medium antiblock. Films produced with this re.. |
|||
Dart Drop | 9.84 g/micron | 250 g/mil | ASTM D1709 |
Westlake Hifor Xtreme SC74842 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74842 polymer is a high strength and good clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. Films produced wit.. |
|||
Dart Drop | 9.84 g/micron | 250 g/mil | ASTM D1709 |
Westlake Hifor Xtreme SC74845 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74845 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and high antiblock. Films produced with this resi.. |
|||
Dart Drop | 9.84 g/micron | 250 g/mil | ASTM D1709 |
Huntsman PE1451 EVA Film Extrusion
(discontinued **) 4.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |