Polymer Property : Dart Drop = 175 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 6.89 g/micron
175 g/mil
ASTM D1709
ExxonMobil Exceed™ 3518 GA Premium Cast Film Resin  (discontinued **)
Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. ..
Dart Drop 6.89 g/micron
175 g/mil
ASTM-D1709
Westlake Elevate™ EB591 9% EVA Copolymer
Westlake EB591 resin is a 9% EVA copolymer designed for films that require excellent toughness and good heat sealing characteristics. This Kosher compliant resin has excellent low temperature brittl..
Dart Drop 6.89 g/micron
175 g/mil
ASTM D1709A
Westlake Mxsite LC78104 Polyethylene
Mxsite LC78104 polyethylene is recommended for the skin layers of cast stretch film. It will provide a very aggressive cling force in both a stretched and unstretched condition. The excellent cling ..
Dart Drop 6.89 g/micron
175 g/mil
ASTM D1709A
ExxonMobil Exceed™ 4518PA Premium Cast Film Resin
Exceed 4518PA resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 4518PA resin have outstanding tensile properties and impact and puncture toughness..
Dart Drop 6.90 g/micron
175 g/mil
Dow DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2056 Polyethylene resin is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer. It complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 ..
Dart Drop 6.89 g/micron
175 g/mil
ASTM D1709
ExxonMobil Exceed™ 3518 CB Premium Cast Film Resin
Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. ..
Dart Drop 6.89 g/micron
175 g/mil
ASTM D1709
ExxonMobil Exceed™ 3518 PA Premium Cast Film Resin
Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. ..
Dart Drop 6.90 g/micron
175 g/mil
ASTM D1709A
Westlake Hifor Xtreme SC74860-F Polyethylene  (discontinued **)
Hifor Xtreme Polyethylene SC74860-F is recommended for the core layer of cast stretch film. It provides excellent clarity and ultimate stretch values higher than the more conventional 2.0-2.5 MI cas..