Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 17.7 g/micron | 450 g/mil | Blown Film at 1 mil; ASTM D-1709 |
Chevron Phillips MarFlex® 7105DL Polyethylene; LLDPE
(discontinued **) Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a.. |