Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 15.0 g/micron | 381 g/mil | ASTM D1709A |
Lotte Chemical Titan TITANCEED® mL216 Linear low density polyethylene resin
(discontinued **) Titanceed® mL216 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt.. |
|||
Dart Drop | 15.0 g/micron | 380 g/mil | ASTM D4272 |
LyondellBasell Ultrathene® UE672006 Ethylene Vinyl Acetate Copolymer, Film Grade Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w.. |
|||
Dart Drop | 15.0 g/micron | 380 g/mil | ASTM D4272 |
LyondellBasell Ultrathene® UE672102 Ethylene Vinyl Acetate Copolymer, Film Grade Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w.. |
|||
Dart Drop | 15.0 g/micron | 380 g/mil | ASTM D4272 |
LyondellBasell Ultrathene® UE672317 Ethylene Vinyl Acetate Copolymer, Film Grade Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w.. |