Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 5.04 g/micron | 128 g/mil | F50; ASTM D1709 |
ExxonMobil Escorene® CR-5810 EVA Resin, for High Cling Stretch Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A tackified Ethylene Vinyl Acetate resin for blown or cast stretch film.Applications: Packing films (cling). Data for film properties below based o.. |
|||
Dart Drop | 5.04 g/micron | 128 g/mil | ASTM D1709 |
Westlake EF602 Low Density Polyethylene Westlake EF602 is a fractional melt LDPE with excellent toughness. It is suggested in heavy duty films and shipping sacks, and in industrial shrink applications. It can be used as a bubble stabilize.. |