Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 4.92 g/micron | 125 g/mil | ASTM D1709 |
Westlake EF403 Low Density Polyethylene WESTLAKE polyethylene EF403 is a fractional melt low-density formulation suggested for use in clarity shrink applications. This LDPE formula exhibits excellent skrinkability, and has very good optic.. |
|||
Dart Drop | 4.92 g/micron | 125 g/mil | ASTM D1709 |
Westlake EF403 Low Density Polyethylene WESTLAKE polyethylene EB403 is a fractional melt low-density formulation suggested for use in clarity shrink applications. This LDPE formula exhibits excellent shrinkability, and has very good optic.. |
|||
Dart Drop | 4.92 g/micron | 125 g/mil | ASTM D1709 |
Westlake EF603 Low Density Polyethylene Westlake EF603 is a LDPE resin with excellent toughness and processability. It is suggested in heavy duty films and medium duty shrink applications. It can be used as a bubble stabilizer in LLDPE ri.. |
|||
Dart Drop | 4.92 g/micron | 125 g/mil | ASTM D1709 |
Westlake EF606 Low Density Polyethylene Westlake EF606 is a LDPE resin suggested for use in multiwall and general purpose liners, and for use as a blend resin in general purpose packaging applications. It has excellent processability, and.. |
|||
Dart Drop | 4.92 g/micron | 125 g/mil | Blown Film at 1 mil; ASTM D-1709 |
Chevron Phillips MarFlex® 7308DK Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD.. |
|||
Dart Drop | 4.92 g/micron | 125 g/mil | Blown Film at 1 mil; ASTM D-1709 |
Chevron Phillips MarFlex® 7308DL Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD.. |
|||
Dart Drop | 4.92 g/micron | 125 g/mil | Blown Film at 1 mil; ASTM D-1709 |
Chevron Phillips MarFlex® 7308FK Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processabilityIncreased stiffnessGood toughnessUse alone or in blends with LDPE o.. |
|||
Dart Drop | 4.92 g/micron | 125 g/mil | ASTM D1709 |
ExxonMobil Pax-Plus™ 3208 Blown Film Resin Pax-Plus 3208 is a rubber modified high density polyethylene film resin offering good physical properties with ease of processing. It exhibits toughness, stress crack resistance and low WVTR.Inform.. |
|||
Dart Drop | 4.92 g/micron | 125 g/mil | ASTM D1709 |
Braskem LQ 0518/21 AF LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Coextruded film for automatic packaging (FFS). Information provided by Braskem |