Polymer Property : Dart Drop = 119 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 4.70 g/micron
119 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips 7109DT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, No Slip, No Antiblock Version of 7109T with Process Aid, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or ble..
Dart Drop 4.70 g/micron
119 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips 7109LT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, High Antiblock Version of 7109TCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPEApplications:Ind..
Dart Drop 4.70 g/micron
119 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips 7109T LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industrial Liners, Stretch Wrap, Garment Bags..
Dart Drop 4.70 g/micron
119 g/mil
F-50 at 26 in.; ASTM D1709
Chevron Phillips 7109D Linear low density polyethylene blown film resin  (discontinued **)
Resin Type: linear low density polyethylene, hexene copolymer, no slip, no antiblock version of 7109 with process aid, cast/blown resinCharacteristics: good stiffness at thin gauges, good drawdown, ..
Dart Drop 4.70 g/micron
119 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips 7109DJT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, Medium Antiblock, Processing Aid Version of 7109T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended w..