Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 4.50 g/micron | 114 g/mil | ASTM D1709 |
SABIC 518N Linear Low Density Polyethylene for Blown Film Product Description: 548N is a fractional melt index Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resin yield outstanding toug.. |
|||
Dart Drop | 4.50 g/micron | 114 g/mil | ASTM D 1709/A |
NOVA Chemicals Surpass® FPs225-A Octene Copolymer sLLDPE Film Resin FPs225-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |
|||
Dart Drop | 4.50 g/micron | 114 g/mil | ASTM-D1709 (Method B) |
Braskem TN2020 EVA General Film Copolymer TN2020 is an Ethylene-Vinyl Acetate (EVA) copolymer developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Multilayer structures.. |
|||
Dart Drop | 4.50 - 29.0 g/micron | 114 - 737 g/mil | Average value: 10.5 g/micron Grade Count:20 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum.. |