Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 1.97 g/micron | 50.0 g/mil | ASTM D1709 |
Huntsman PE1037 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Medium clarity packaging film and good draw down characteristics.Applications: Film extrusion: general purpose packaging and film applications.FDA Notes: Con.. |
|||
Dart Drop | 1.97 g/micron | 50.0 g/mil | ASTM D1709 |
Huntsman PE1044 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA reg.. |
|||
Dart Drop | 1.97 g/micron | 50.0 g/mil | ASTM D1709 |
Huntsman PE1065 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA regu.. |
|||
Dart Drop | <= 1.97 g/micron | <= 50.0 g/mil | ASTM D1709 |
Chevron Phillips mPact™ D449 HDPE Blown Film Resin
(discontinued **) Resin Type: High density, hexene copolymerCharacteristics: excellent clarity, high gloss, good modulus, process with LLDPE setup, optimum clarity when used as an individual layer.Applications: overw.. |
|||
Dart Drop | 1.97 - 30.0 g/micron | 50.0 - 762 g/mil | Average value: 6.87 g/micron Grade Count:116 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Dart Drop | <= 1.97 g/micron @Thickness 0.0254 mm |
<= 50.0 g/mil @Thickness 0.00100 in |
ASTM D1709A |
Total 9458 HDPE Film Grade Medium molecular weight grade. Excellent bubble stability, good compatibility with LDPE and LLDPE, good heat resistance, high stiffness and tensile strength.Applications: Release liners, Stand-up ba.. |
|||
Dart Drop | 1.97 g/micron | 50.0 g/mil | ASTM D1709 |
Chevron Phillips MarFlex® 9656 HDPE Blown Film Resin Resin Type: high density, linear polyethylene.Characteristics: copolymerization enhances film toughness, good drawdown, density level gives good machinability, blend well with LLDPEApplications: not.. |
|||
Dart Drop | 1.97 g/micron | 50.0 g/mil | ASTM D1709 |
ExxonMobil Escorene® LD 713.93 Cast Film Resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhbits very high impact strength, hihg clarity, and excellent heat sealabilityAvailability: Latin.. |
|||
Dart Drop | 1.97 g/micron | 50.0 g/mil | ASTM D1709 |
Braskem BC 818 LDPE Extrusion Coating Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Extrusion coating. Information provided by Braskem |
|||
Dart Drop | 1.97 g/micron | 50.0 g/mil | ASTM D1709 |
Huntsman PE1059 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down and good processability.Applications: Film extrusion: non-abrasive packaging applications.FDA Notes: Conforms to FDA regulation 21 CFR 177.. |
|||
Dart Drop | 1.97 g/micron | 50.0 g/mil | ASTM D1709 |
Huntsman PE1076 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrap packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (.. |
|||
Dart Drop | 1.97 g/micron | 50.0 g/mil | ASTM D1709 |
Huntsman PE1078 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrap packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (.. |