Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 1.60 g/micron | 40.6 g/mil | ASTM D 1709/A |
NOVA Chemicals Surpass® FPs236-A Octene sMDPE Film Resin FPs236-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPs236-.. |
|||
Dart Drop | 1.60 g/micron | 40.6 g/mil | at -18°C; ASTM D1709 |
Eastman 9921 PET Film
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Dart Drop | 1.60 g/micron | 40.6 g/mil | F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips 6120 LLDPE Cast/Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applicationsAp.. |
|||
Dart Drop | 1.60 g/micron | 40.6 g/mil | F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips 5497 LDPE High Clarity, Bakery Packaging Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Openability, Suited for High Speed Converting, Good Clarity. Slip 1000 ppm. Antiblock 10000 ppm.Applications:Bakery Film, Bread BagsProcessing Con.. |
|||
Dart Drop | 1.60 g/micron | 40.6 g/mil | 38mm Dart, 66mm height; ASTM D1709 |
Reliance Industries Relene F56003 Polyethylene Relene F56003 is a High Density Polyethylene grade suitable for producing blown parts with excellent drawdown and paper like feel. It is recommended for making carrier bags and coextruded film stru.. |
|||
Dart Drop | 1.60 g/micron | 40.6 g/mil | |
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2027A Polyethylene resin is a higher density polymer for cast film applications with improved stiffness. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2(a) for food contact appli.. |
|||
Dart Drop | 1.60 g/micron | 40.6 g/mil | |
Dow HDPE 05862N High Density Polyethylene Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical. |
|||
Dart Drop | 1.60 g/micron | 40.6 g/mil | at -18°C; ASTM D1709 |
Eastman 9921W PET Film
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Dart Drop | 1.60 g/micron | 40.6 g/mil | |
Dow LDPE 535I Low Density Polyethylene, Liner Grade DOW LDPE 535I resin is a barefoot general purpose liner resin with medium clarity for medium modulus packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for.. |