Polymer Property : Dart Drop = 1.16 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 1.16 g/micron
29.5 g/mil
F 50; ASTM D1709/A
NOVA Chemicals Sclair® 19C Homopolymer HDPE Film Resin
Film Properties. Features: Good stiffness, good barrier, high clarity, narrow MWD.Applications: Lamination, co-extrusion.Data provided by the manufacturer.