Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 900 g | 900 g | ASTM D1922 |
LyondellBasell Petrothene® GA601031 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
Elmendorf Tear Strength TD | 900 g | 900 g | ASTM D1922 |
LyondellBasell Petrothene® GA601032 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
Elmendorf Tear Strength TD | 900 g | 900 g | ASTM D1922 |
LyondellBasell Petrothene® GA601033 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
Elmendorf Tear Strength TD | 900 g | 900 g | ASTM D1922 |
LyondellBasell Alathon® L5885 High Density Polyethylene ApplicationsALATHON L 5885 is a medium molecular weight high density homopolymer for use in blown film applications. Typical applications include those low WVTR requirements.Regulatory StatusL 5855.. |
|||
Elmendorf Tear Strength TD | 900 g | 900 g | ASTM D1922 |
LyondellBasell Petrothene® GA601030 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |