Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 700 g | 700 g | |
Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2036A Polyethylene resin is a cast film polymer having improved thermal stability for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a for food .. |
|||
Elmendorf Tear Strength TD | 700 g | 700 g | ASTM D1922 |
Dow DOWLEX™ 2020G Linear Low Density Polyethylene DOWLEX™ 2020G is perfect for high strength consumer trash bags/liners. This product can be used in other applications that require toughness and also offers great melt strength for high throughput.. |
|||
Elmendorf Tear Strength TD | 700 g | 700 g | ASTM-D1922 |
Braskem TU3001 LDPE Blown Film Extrusion Polyethylene TU3001 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties, and good processability. These qualities ensure the production of films with uniform thicknes.. |
|||
Elmendorf Tear Strength TD | 700 g | 700 g | ASTM D1922 |
M. Holland Company MAGMA® LM203-C LLDPE
(discontinued **) Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland. |