Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 690 g | 690 g | ASTM D1922 |
LyondellBasell Plexar® PX5125 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE ApplicationsPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copo.. |
|||
Elmendorf Tear Strength TD | 690 g | 690 g | ASTM D1922 |
Dow DOWLEX™ 2056G Linear Low Density Polyethylene Improved thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |