Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 640 g | 640 g | |
Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045.02 Polyethylene resin is a premier film resin for general packaging applications ranging from heavy duty applications to high speed, thin gauge applications. It contains high level of .. |
|||
Elmendorf Tear Strength TD | 640 g | 640 g | |
Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045.11 Polyethylene resin is a premier film resin for general purpose packaging applications, ranging from heavy duty applications to high speed, thin gauge applications. It contains high .. |
|||
Elmendorf Tear Strength TD | 640 g | 640 g | Method B; ASTM D1922 |
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-7002 NT 7 is an ethylene-hexene-1 copolymer, design.. |
|||
Elmendorf Tear Strength TD | 640 g | 640 g | ASTM D1922 |
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 0.6 mil Film, Stiff
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |