Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 510 g | 510 g | ISO 6383-2 |
EMS-Grivory Grivory® HB 5299 HV PA* Product description: Grivory HB 5299 HV is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. HV indicates high viscosity, sui.. |
|||
Elmendorf Tear Strength TD | 510 g | 510 g | ISO 6383-2 |
EMS-Grivory Grivory® HB5299 PA* Product description: Grivory HB 5299 is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. Excellent oxygen and carbon dioxide.. |
|||
Elmendorf Tear Strength TD | 510 g | 510 g | |
Dow Primacor® 1430 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Elmendorf Tear Strength TD | 510 g | 510 g | gF; ASTM D1922 |
Braskem Green PE SLH118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLH118 is a Linear Low Density Polyethylene, copolymer of hexene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process.. |
|||
Elmendorf Tear Strength TD | 510 g | 510 g | ASTM 1922 |
Braskem LH 118 LLDPE Blown Film Extrusion Polyethylene Description: LH118 is a Linear Low Density Polyethylene, copolymer of hexene-1, produced by Spherilene process. Developed for blown film extrusion in blends with polyethylenes. Films obtained with t.. |
|||
Elmendorf Tear Strength TD | 510 g | 510 g | gF; ASTM D1922 |
Braskem LH118 Blown Film Extrusion Linear Low Density Polyethylene Stretch films; Liners; LDPE and HDPE blends; Packages for general use.Information provided by Braskem. |