Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 490 g | 490 g | ASTM D 1922 |
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Elmendorf Tear Strength TD | 490 g | 490 g | ASTM D1922 |
M. Holland Company MAGMA® LM115-B LLDPE
(discontinued **) Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Elmendorf Tear Strength TD | 490 g | 490 g | ASTM D-1922 |
Bapolene® 122B Polyethylene, Film Grade Bapolene LL122B is a general purpose LLDPE for blown film extrusion. This resin offers excellent tensile and toughness properties. Contains no slip and no antiblock additives. This product meets .. |
|||
Elmendorf Tear Strength TD | 490 g | 490 g | ASTM D1922 |
Huntsman Rexell® M3109 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer and FDA compliant.Features: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, multi-layer syste.. |
|||
Elmendorf Tear Strength TD | 490 - 900 g | 490 - 900 g | Average value: 729 g Grade Count:12 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |