Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 461 g | 461 g | ASTM D1922 |
Dow AFFINITY™ PF 1146G Polyolefin Plastomer (POP) AFFINITY™ PF 1140G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for high speed packaging applications requiring low seal initiation temperature and good machina.. |