Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 460 g | 460 g | ASTM D1922 |
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin; 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have.. |
|||
Elmendorf Tear Strength TD | 460 g | 460 g | ASTM D1922A |
LyondellBasell Montell 12C01G2 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f.. |
|||
Elmendorf Tear Strength TD | 460 g | 460 g | ASTM D1922A |
LyondellBasell Montell 12C01G3 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, low antiblockApplications: .. |
|||
Elmendorf Tear Strength TD | 460 g | 460 g | ASTM D1922A |
LyondellBasell Montell 12C01G4 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, high slip, medium antiblockApplicati.. |
|||
Elmendorf Tear Strength TD | 460 g | 460 g | ASTM D1922A |
LyondellBasell Montell 12C01G5 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl.. |
|||
Elmendorf Tear Strength TD | 460 g | 460 g | ASTM D1922 |
Iran Petrochemical (PCC) LL22501 Linear Low Density Polyethylene 22501 is a high stiffness LLDPE blown film grade designed for applications requiring good optical properties even at low extrusion temperature. This resin combines ease of processing with low gels a.. |
|||
Elmendorf Tear Strength TD | 460 g | 460 g | ASTM D1922 |
ExxonMobil Exceed™ 2018HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018HA is a metallocene Catalyzed ethylene-hexene copolymer. Films made from Exceed 2018HA have outstanding tensile, impact strength, and puncture. These superior strengt.. |
|||
Elmendorf Tear Strength TD | 460 g | 460 g | ASTM D1922 |
ExxonMobil Exceed™ 4518PA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 4581PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 4581PA have outstanding tensile properties and impact and puncture toughness. These superior prope.. |
|||
Elmendorf Tear Strength TD | 460 g | 460 g | ASTM D1922 |
ExxonMobil LLDPE LL 1001.32 Linear Low Density Polyethylene Resin Product Description: LL 1001.32 is a butane LLDPE resin. Films made from LL 1001.32 have very good tensile and toughness properties.Availability: Latin America, North America and South America Addit.. |
|||
Elmendorf Tear Strength TD | 460 g | 460 g | Unspecified film thickness |
Dow Elite® 5200 Linear Low Density Polyethylene 5200 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. This resin offers high impact strength and good puncture resistance at moderate stretch levels for .. |
|||
Elmendorf Tear Strength TD | 460 g | 460 g | ASTM D1922 |
ExxonMobil Escorene™ 768.MJ Blown Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 768.MJ is a low gel 26.2% vinyl acetate copolymer designed for film and compounding applications. This resin provides very low modulus films with high tensile .. |
|||
Elmendorf Tear Strength TD | 460 g | 460 g | gF; ASTM D1922 |
Braskem Flexus® 7200 Cast Film Extrusion Polyethylene Description: Braskem Flexus7200 is a Linear Low Density Polyethylene, metallocene ethylene-hexene copolymer, produced by gas fase process. It was specially designed to provide outstanding processing.. |
|||
Elmendorf Tear Strength TD | 460 g | 460 g | ASTM-D1922 |
Braskem LL6802N LLDPE Blown Film Extrusion Polyethylene Copolymer LL6802N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing aid .. |
|||
Elmendorf Tear Strength TD | 460 g | 460 g | ASTM D1922 |
ExxonMobil Exceed™ 3518CB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 3518CB is a metallocene ethylene-hexene copolymer. Films made of Exceed 3518CB grade have outstanding tensile, impact and puncture resistance properties. Furthermore, the.. |
|||
Elmendorf Tear Strength TD | 460 g | 460 g | ASTM D1922 |
ExxonMobil Exceed™ 4518CB Metallocene Polyethylene Resin Product Description: Exceed 4518 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 4518 have outstanding tensile properties and impact and puncture toughness. These superior p.. |