Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 430 g
430 g
ASTM D 1922
NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin
FPs016-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem..
Elmendorf Tear Strength TD 430 g
430 g
ASTM D1922
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength propertie..
Elmendorf Tear Strength TD 430 g
430 g
ASTM D1922
ExxonMobil Exceed™ 1023CA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1023CA is a metallocene ethylene-hexene copolymers. The slightly higher stiffness of Exceed 1023CA makes it easier to process on certain filling machinery, whilst still k..
Elmendorf Tear Strength TD 430 g
430 g
ASTM D1922
ExxonMobil Exceed™ 1327ED Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1327ED is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327ED is fully formula..
Elmendorf Tear Strength TD 430 g
430 g
ASTM D1922
ExxonMobil LLDPE LL 1002YB Cast Linear Low Density Polyethylene Resin
Product Description: LL 1002YB is an LLDPE resin designed for cast films. It offers high gloss and excellent drawdown in both blown and cast film applications. LL 1002YB may also be used as a blend ..
Elmendorf Tear Strength TD 430 g
430 g
ASTM D1922
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength proper..
Elmendorf Tear Strength TD 430 g
430 g
ASTM-D1922
Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer
The FC31D resin is a linear low-density polyethylene, copolymer of butene -1, produced by the solution process for blow film extrusion. It has excellent mechanical properties, especially hot tack. I..