Polymer Property : Elmendorf Tear Strength TD = 320 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 320 g
320 g
ASTM D1922
SABIC 218 Series Linear Low Density Polyethylene for Blown Film
Product Description: 218 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. They are easy to process giving good tensile properties, impact strength a..
Elmendorf Tear Strength TD 320 g
320 g
ASTM D 1922
NOVA Chemicals Novapol® TF-0438-E Hexene LMDPE Film Resin
TF-0438-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur..
Elmendorf Tear Strength TD 320 g
320 g
ASTM D1922
Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene
09X02 is a high performance LLDPE (HP-LLDPE) cast film grade combines ease of processing with low gels and good film strength. Its excellent stretchability makes this grade particularly suited for s..
Elmendorf Tear Strength TD 320 g
320 g
ASTM D1922
ExxonMobil Optema® TC-110 Blown Ethylene Methyl Acrylate
Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elast..
Elmendorf Tear Strength TD 320 g
320 g
ASTM-D1922
Braskem LF320 LLDPE Cast Film Extrusion Polyethylene Copolymer
LF320 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It was developed for cast film extrusion. Films obtained with this product show a good processin..