Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
SABIC 726 Series Linear Low Density Polyethylene for Blown Film
Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher ..
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
LyondellBasell Petrothene® NA420127 Low Density Polyethylene  (discontinued **)
ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel..
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
ExxonMobil Escorene® LD-103 LDPE Industrial Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer industrial film resin with excellent toughness. LD-103 has a low melt index which gives excellent impact strength and melt strength o..
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
LyondellBasell Petrothene® NA340141 Low Density Polyethylene
ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea..
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
LyondellBasell Petrothene® NA340163 Low Density Polyethylene
ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea..
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
LyondellBasell Petrothene® NA340185 Low Density Polyethylene, Film Extrusion Grade
PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include hea..
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
LyondellBasell Petrothene® NA340212 Low Density Polyethylene, Film Extrusion Grade
PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include hea..
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
LyondellBasell Petrothene® NA420000 Low Density Polyethylene
ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel..
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
LG Chemical SEETEC EF221 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical Properties Additives: Antiblocking agent, Slip AgentApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
LyondellBasell Petrothene® NA340013 Low Density Polyethylene
ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea..
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
LyondellBasell Petrothene® NA426225 Low Density Polyethylene, Film Extrusion Grade
PETROTHENE NA426 is a series of LDPE/EVA copolymer resins for high impact and clarity packaging film. These resins exhibit excellent a broad range of extrusion conditions. Well-balanced films with e..
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
LyondellBasell Petrothene® NA480145 Low Density Polyethylene
ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low..
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
LyondellBasell Petrothene® NA480177 Low Density Polyethylene
ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low..
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
LyondellBasell Petrothene® NA480178 Low Density Polyethylene
ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low..
Elmendorf Tear Strength TD 250 g
250 g
Dow LDPE 640I Low Density Polyethylene, Liner Film Grade
DOW LDPE 640I resin is a barefoot general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. This material complies with U.S.FDA regulation 21 CFR ..
Elmendorf Tear Strength TD 250 g
250 g
Dow LDPE 641I Low Density Polyethylene, Liner Film Grade
DOW LDPE 641I resin is a general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. It contains medium levels of slip additive and low levels of an..
Elmendorf Tear Strength TD 250 g
250 g
ASTM-D1922
Braskem TN7006 LDPE Blown Film Extrusion Polyethylene
TN7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a great combination of mechanical, optical, and stiffness properties. TN7006 h..
Elmendorf Tear Strength TD 250 g
250 g
ASTM-D1922
Braskem TS7006 LDPE Blown Film Extrusion Polyethylene
TS7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a combination of mechanical, optical, and stiffness properties. TS7006 has a l..
Elmendorf Tear Strength TD 250 g
250 g
ISO 6283-2
Carmel Olefins IPETHENE® 111 Low Density Polyethylene
IPETHENE® 111 is a low density polyethylene extrusion grade, contains no additives. It exhibits a good balance between mechanical and optical properties. APPLICATIONS IPETHENE® 111 is used to pr..
Elmendorf Tear Strength TD 250 g
250 g
ISO 6283-2
Carmel Olefins IPETHENE® 113 Low Density Polyethylene
IPETHENE® 113 is a general purpose low density polyethylene film extrusion grade. It contains medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between me..
Elmendorf Tear Strength TD 250 g
250 g
ISO 6283-2
Carmel Olefins IPETHENE® 320 Low Density Polyethylene
IPETHENE® 320 is a general purpose low density polyethylene film extrusion grade, containing no additives. It exhibits good mechanical and optical properties. APPLICATIONS IPETHENE® 320 is mainl..
Elmendorf Tear Strength TD 250 g
250 g
ISO 6283-2
Carmel Olefins IPETHENE® 322 Low Density Polyethylene
IPETHENE® 322 is a general purpose low density polyethylene film extrusion grade. It contains a medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between ..
Elmendorf Tear Strength TD 250 g
250 g
ISO 6283-2
Carmel Olefins IPETHENE® 323 Low Density Polyethylene
IPETHENE® 323 is a general purpose low density polyethylene film extrusion grade. It contains a high level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between me..
Elmendorf Tear Strength TD 250 g
250 g
Dow LDPE 607A Low Density Polyethylene, High Clarity Blown Film Grade
DOW LDPE 607A resin is a fully formulated high clarity blown film resin for thin gauge optical applications, such as bakery film. It contains medium levels of slip additive and low levels of antiblo..