Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 190 g | 190 g | ASTM D1922 |
ExxonMobil Escorene™ FL 00209 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00209 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (518°F) may cause resin degradation. Machines should always b.. |
|||
Elmendorf Tear Strength TD | 190 g | 190 g | ASTM D1922 |
ExxonMobil Escorene™ FL 00212 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00212 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 260°C (500°F) may cause resin degradation. Machines should always b.. |
|||
Elmendorf Tear Strength TD | 190 g | 190 g | ASTM D1922 |
ExxonMobil LD 105.BR Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Elmendorf Tear Strength TD | 190 g | 190 g | gF; ASTM D1922 |
Braskem Green PE SLL218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL218 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for cast film extrusion. Films obtained with this product show a good processing performance balanced with .. |
|||
Elmendorf Tear Strength TD | 190 g | 190 g | ASTM D1922 |
Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Stretch film; shrink film; "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem |
|||
Elmendorf Tear Strength TD | 190 g | 190 g | ASTM D1922 |
Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene Description: LL218 is a Linear Low Density Polyethylene, copolymer of butene-1, produced by Spherilene process. Developed for cast film extrusion. Films obtained with this product show a good proces.. |
|||
Elmendorf Tear Strength TD | 190 g | 190 g | gF; ASTM D1922 |
Braskem LL218 Cast Film Extrusion Linear Low Density Polyethylene Stretch films; Liners; LDPE and HDPE blends; Packages for general use.Information provided by Braskem. |