Polymer Property : Elmendorf Tear Strength TD = 170 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 170 g
170 g
Eastman 1840F Polyethylene  (discontinued **)
Polyethylene 1840F is a low-density formulation with no slip or antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is characterized by..
Elmendorf Tear Strength TD 170 g
170 g
Blown; ASTM D1922
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..
Elmendorf Tear Strength TD 170 g
170 g
Blown; ASTM D1922
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..
Elmendorf Tear Strength TD 170 g
170 g
ASTM D1922
ExxonMobil LDPE LD 152BW Low Density Polyethylene Resin
Product Description: LD 152BW is an LDPE grade offering an excellent combination of optical properties and stiffness. The 2.2 MI makes it ideal for blowing thicker films.Availability: Africa & Middl..
Elmendorf Tear Strength TD 170 g
170 g
ASTM D1922
ExxonMobil LLDPE LL 3404.48 Linear Low Density Polyethylene Resin
Product Description: LL 3404.48 is a hexane medium density polyethylene cast film grade for applications requiring high strength and high stiffness. Films produced from this resin exhibit good tensi..
Elmendorf Tear Strength TD 170 g
170 g
Dow LDPE 530A Low Density Polyethylene, Blown Film Grade
DOW LDPE 530A resin, is a general purpose barefoot blown film extrusion resin with excellent drawdown and processability for packaging applications. This material complies with U.S.FDA regulation 21..
Elmendorf Tear Strength TD 170 g
170 g
Dow LDPE 493A Low Density Polyethylene, Film Grade
DOW LDPE 493A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 493A resin can be blended with most linear low density..