Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
SABIC HP4023W Low Density Polyethylene for Blown Film
Product Description: HP4023W is a Low Density Polyethylene grade suitable for producing general purpose films and contains slip and antiblock additives. It yields excellent processability with goo..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LD 051.LJ Shrink Film Resin  (discontinued **)
LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LD 051.LT Shrink Film Resin  (discontinued **)
LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D 1922
Total Finathene® 2344 HDPE film  (discontinued **)
Applications: Trash can liners, merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
LyondellBasell Petrothene® M2520FN Low Density Polyethylene
ApplicationsPETROTHENE M 2520 is a film grade resin that exhibits excellent optics, good gloss and good bubble stability. A typical application for this resin is high clarity packaging. Regulatory..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D 1922
Total 1285 HDPE film
Applications: T-shirt sacks, trash can liners, merchandise bags, coex applicationsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D 1922
Total 2285 HDPE Bimodal Film Resin
Applications: T-shirt sacks, trash can liners, merchandise bags, multi-wall liner, deli wrapInformation provided provided by Total Petrochemicals.
Elmendorf Tear Strength TD 120 g
120 g
ASTM D 1922
Total 2287 HDPE Bimodal Film Resin
Broad molecular weight distribution. Designed for die build-up sensitive equipmentApplications: T-shirt sacks, trash can liners, merchandise bags, deli wrapInformation provided provided by Total Pe..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil Escorene™ LD 730.09 Blown Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 730.09 is a 17.2% vinyl acetate copolymer film resin. LD 730.09 is designed to have superior strength and toughness combined with excellent optics and sealing ..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LD 051.LQ Shrink Film Resin
L Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding pr..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LD 123.LN General Purpose Clarity Film Resin
Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America ..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LDPE LD 051.LQ Low Density Polyethylene Resin
Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding proc..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LDPE LD 100.BW Low Density Polyethylene Resin
Product Description: LD 100.BW is a LDPE grade, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.Ava..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LDPE LD 100AC Low Density Polyethylene Resin
Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LDPE LD 100BR Low Density Polyethylene Resin
Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin
Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LDPE LD 104BR Low Density Polyethylene Resin
Product Description: LD 104BR is an LDPE grade, which offers good optical properties combined with increased stiffness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antibloc..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LDPE LD 123.LN Low Density Polyethylene Resin
Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America ..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LDPE LD 158BW Low Density Polyethylene Resin
Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel ..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LDPE LD 158JD Low Density Polyethylene Resin
Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel ..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin
Product Description: LD 165BW1 is a fractional melt index LDPE, with medium optical properties.Availability: Latin America, North America and South America Applications: Agricultural FilmBlend Part..
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
ExxonMobil LDPE LD 313.NF Low Density Polyethylene Resin
Product Description: LD 313.NF is a 3 % vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopoly..