Polymer Property : Tensile Strength, Ultimate = 990 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 6.83 MPa
990 psi
post cured- 4 hours at 204°C
Multibase SILASTIC® C7-4550 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 6.83 MPa
990 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 281-87MED Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad..