Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.80 - 11.7 MPa
1420 - 1700 psi
Average value: 10.9 MPa Grade Count:4
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade". Each property range of values reported is min..
Tensile Strength, Ultimate 9.80 MPa
1420 psi
ASTM D638
ExxonMobil Escorene® MV-02528 EVA Copolymer, Adhesive and Sealant Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants.
Tensile Strength, Ultimate 9.80 MPa
1420 psi
Dow DOWLEX™ 2553 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2553 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and impact strength with excellent stiffness for hou..
Tensile Strength, Ultimate 9.80 MPa
1420 psi
508 mm/min; ASTM D638
Dow Engage® 8452 Polyolefin Elastomer
Description: Engage® 8452 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent toughness, softness, and optical properties. It has excellent compatibility with other polyolefin..
Tensile Strength, Ultimate 9.80 - 37.3 MPa
1420 - 5410 psi
Average value: 23.1 MPa Grade Count:25
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..