Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 41.4 - 61.0 MPa | 6000 - 8850 psi | Average value: 49.7 MPa Grade Count:22 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |