Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 6.03 MPa | 875 psi | post cured- 4 hours at 204°C |
Multibase SILASTIC® C7-4565 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Ultimate | 6.03 MPa | 875 psi | |
Momentive Performance Materials RTV6445 White Adhesive Sealant, Non-Corrosive High Strength Paste One-part heat cure. Typical uses: Thermal barrier for automotive parts. Fabric seam seal.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materia.. |
|||
Tensile Strength, Ultimate | 6.03 MPa | 875 psi | Cured property; ASTM D412 |
Aptek 2205 A/B Low modulus urethane stacking compound APTEK 2205-A/B is a thixotropic, two component, electrically insulating, low modulus urethane system designed for the staking of electrical/electronic components to printed circuit boards. Although.. |